| Tool | File |
|---|---|
| Problem | Burrs on the inside and outside edges of the pipe were manually removed by filing. Time-consuming and inefficient work. Finish quality was not consistent. |
| Tool | XEBEC Brush Surface (A11-CB25M) |
|---|---|
| Result | Fix and put 12 pipes together with a jig and deburr them all at once. Achieved efficient automatic deburring in a shorter time. Edge shapes became uniform and finish quality was improved. |

| Industry | General Machinery |
|---|---|
| Part name | Pipe (Aluminum) |
| Material type | Aluminum alloy |
| Machining process | Cutting processing |
| Tool | XEBEC Brush Surface (A11-CB25M) |
|---|---|
| Details of processing | Deburring the section after cutting process |
| Rotational speed (min⁻¹) | 4000 |
| Feed rate (mm/min) | 3000 |
| Depth of cut (mm) | 1.0 |
| Machining time (sec) | – |