Turbine blade

Before
Tool

File

Problem

Deburring caused unstable edge quality. Recovering process was required.

After
Tool

XEBEC Brush Surface (A11-CB25M)

Result

By the introduction of automated deburring, stable quality with even edge shape realized.

Workpiece information
Industry

Aerospace

Part name

Turbine blade

Material type

Stainless steel

Machining process

Ball end mill processing

Processing conditions
Tool

XEBEC Brush Surface (A11-CB25M)

Details of processing

Deburring after ball-end milling process

Rotational speed (min⁻¹)

1,000

Feed rate (mm/min)

1,000

Depth of cut (mm)

0.3

Machining time (sec)

XEBEC Brush™ Surface