| Tool | Abrasive-impregnated nylon brush |
|---|---|
| Problem | Deformation of nylon brush shape occurred in mass production process. It caused unstable quality due to insufficient deburring performance and burr remaining. |

| Tool | XEBEC Brush for Surface (A11-CB40M) |
|---|---|
| Result | No deformation of brush shape in mass production process. Stable cutting parameters with no burrs realized. |

| Industry | Automotive |
|---|---|
| Part name | VCT housing |
| Material type | Sintered metal |
| Machining process | Front cutter processing |
| Tool | XEBEC Brush for Surface (A11-CB40M) |
|---|---|
| Details of processing | Deburring the edge face after milling process |
| Rotational speed (min⁻¹) | 500 |
| Feed rate (mm/min) | 2,000 |
| Depth of cut (mm) | 0.5 |
| Machining time (sec) | – |