| Tool | Wire brush |
|---|---|
| Problem | After deburring process, burrs remained due to complicated shape of workpiece. |

| Tool | XEBEC Brush for Surface (A11-CB40M) |
|---|---|
| Result | No burrs left and finish quality improved. |

| Industry | Automotive |
|---|---|
| Part name | Cooling fin |
| Material type | Aluminum alloy |
| Machining process | Others |
| Tool | XEBEC Brush for Surface (A11-CB40M) |
|---|---|
| Details of processing | Deburring the edge after cutting process |
| Rotational speed (min⁻¹) | 3000 |
| Feed rate (mm/min) | 800 |
| Depth of cut (mm) | 1 |
| Machining time (sec) | – |