Vacuum forming

Before
Tool

Sandpaper

Problem

It was necessary to use multiple types of abrasive papers and it took long time for polishing. Additionally, manual deburring process caused unstable finish quality.

After
Tool

XEBEC Brush Surface (A11-CB25M)

Result

Polishing in a shorter cycle time with stable quality realized.

Workpiece information
Industry

Mold

Part name

Vacuum forming

Material type

Aluminum

Machining process

End mill processing

Processing conditions
Tool

XEBEC Brush Surface (A11-CB25M)

Details of processing

Removal of cutter marks and polishing after end milling process

Spindle speed (min⁻¹)

3,600

Table feed (mm/min)

4,000

Depth of cut (mm)

0.3

Machining time (sec)

XEBEC Brush™ Surface