| Tool | File |
|---|---|
| Problem | Deburring caused unstable edge quality. Recovering process was required. |
| Tool | XEBEC Brush Surface (A11-CB25M) |
|---|---|
| Result | By the introduction of automated deburring, stable quality with even edge shape realized. |

| Industry | Aerospace |
|---|---|
| Part name | Turbine blade |
| Material type | SUS316 |
| Machining process | Ball end mill processing |
| Tool | XEBEC Brush Surface (A11-CB25M) |
|---|---|
| Details of processing | Deburring after ball-end milling process |
| Spindle speed (min⁻¹) | 1,000 |
| Table feed (mm/min) | 1,000 |
| Depth of cut (mm) | 0.3 |
| Machining time (sec) | – |