| Tool | Abrasive-impregnated nylon brush |
|---|---|
| Problem | Burrs remained due to insufficient grinding force of nylon brushes and additional manual deburring process required. |

| Tool | XEBEC Brush for Surface (A11-CB40M) |
|---|---|
| Result | Stable and efficient deburring realized by fully automated deburring with machining centers. |

| Industry | Automotive |
|---|---|
| Part name | Cam cap |
| Material type | ADC12 |
| Machining process | Front cutter processing |
| Tool | XEBEC Brush for Surface (A11-CB40M) |
|---|---|
| XEBEC Brush for Surface (A11-CB40M) | Deburring the matching surface after face milling process. |
| Spindle speed (min⁻¹) | 1350 |
| Table feed (mm/min) | 2000 |
| Depth of cut (mm) | 0.5 |
| Machining time (sec) | – |