| Tool | Abrasive-impregnated nylon brush  | 
								
|---|---|
| Problem | Deformation of nylon brush shape occurred in mass production process. It caused unstable quality due to insufficient deburring performance and burr remaining.  | 
								

| Tool | XEBEC Brush for Surface (A11-CB40M)  | 
								
|---|---|
| Result | No deformation of brush shape in mass production process. Stable cutting parameters with no burrs realized.  | 
								

| Industry | Automotive  | 
								
|---|---|
| Part name | VCT housing  | 
								
| Material type | Sintered metal  | 
								
| Machining process | Front cutter processing  | 
								
| Tool | XEBEC Brush for Surface (A11-CB40M)  | 
								
|---|---|
| Details of processing | Deburring the edge face after milling process  | 
								
| Spindle speed (min⁻¹) | 500  | 
								
| Table feed (mm/min) | 2,000  | 
								
| Depth of cut (mm) | 0.5  | 
								
| Machining time (sec) | –  |